(type IA, 16-sided, diameter 3.10 mm, +70° front anvil)
| Culet size (μm) | Max. pressure (GPa) |
| 80 x 300 | 125-150 |
| 150 x 300 | 100-120 |
| 250 x 300 | 60-70 |
| 250 | 55-60 |
| 300 | 50-55 |
| 350-400 | 40-50 |
| 500 | 20-30 |
| 600 | 15-18 |
| 800 | 5 |
| 1000 | 1 |
All new anvils broken above 80 GPa and/or severely damaged due to laser heating need to be reimbursed. All anvils broken when the above guidelines were not respected also need to be reimbursed.
P01064

Order example for 150 μm x 300 μm (bevelled) anvil:
Diamond anvil, type Ia, Boehler-Almax design, 16-sided, diameter 3.10 mm 70° (X-ray aperture 4θ), culet of 0.15 mm, bevels up to 0.30 mm at 8° , (100)-oriented, low birefringence
Order example for 250 μm anvil:
Diamond anvil, type Ia, Boehler-Almax design, 16-sided, diameter 3.10 mm 70° (X-ray aperture 4θ), culet of 0.25 mm, (100)-oriented, low birefringence
For more information, go to the Boehler Almax website for references.